Analysis of density changes in plutonium observed from accelerated aging using Pu-238 enrichment
[摘要] We present dimensional and density changes in an aging plutonium alloy enriched with 7.3 at.% of Pu-238 and reference alloys of various ages. After 45 equivalent years of aging, the enriched alloys at 35 degrees C have swelled in length by 0.048-0.052% and now exhibit a near linear dimensional increase, without void swelling. Based on X-ray diffraction measurements, the lattice expansion by self-irradiation appears to be the primary cause for dimensional changes during the initial 2-3 years of aging. Following the initial transient, the density change is primarily cause by a constant helium in-growth rate as a result of a-particle decay. Published by Elsevier B.V.
[发布日期] 2007-10-11 [发布机构]
[效力级别] Proceedings Paper [学科分类]
[关键词] delta-Pu(Ga);Pu-238-enriched alloys;plutonium aging;dilatometry [时效性]