Mechanical properties of tungsten alloys with Y2O3 and titanium additions
[摘要] In this research the mechanical behaviour of pure tungsten (W) and its alloys (2 wt.% Ti-0.47 wt.% Y2O3 and 4 wt.% Ti-0.5 wt.% Y2O3) is compared. These tungsten alloys, have been obtained by powder metallurgy. The yield strength, fracture toughness and elastic modulus have been studied in the temperature interval of 25 degrees C to 1000 degrees C. The results have shown that the addition of Ti substantially improves the bending strength and toughness of W, but it also dramatically increases the DBTT. On the other hand, the addition of 0.5% Y2O3, is enough to improve noticeably the oxidation behaviour at the higher temperatures. The grain size, fractography and microstructure are studied in these materials. Titanium is a good grain growth inhibitor and effective precursor of liquid phase in HIP. The simultaneous presence of Y2O3 and Ti permits to obtain materials with low pores presence. (C) 2011 Elsevier B.V. All rights reserved.
[发布日期] 2011-10-01 [发布机构] 
[效力级别]  Proceedings Paper [学科分类] 
[关键词]  [时效性] 
   浏览次数:2      统一登录查看全文      激活码登录查看全文