Self Induced Buoyant Blow Off in Upward Flame Spread on Thin Solid Fuels
[摘要] Upward flame spread experiments were conducted on a thin fabric cloth consisting of 75% cotton and 25% fiberglass. The sample is sandwiched symmetrically with stainless steel plates with the exposed width varying between 2 to 8.8 cm from test to test and >1.5m tall. The bottom edge was ignited resulting in a symmetric two sided flame. For the narrower samples (. 5cm), two sided flame growth would proceed until reaching some limiting value (15-30 cm depending on sample width). Fluctuation or instability of the flame base on one side would initially become visible and then the flame base would retreat downstream and cause extinguishment on one side. Detailed examination of the still images shows that the fuel continues to vaporize from the extinguished side due to the thermally thin nature of the fuel. But, due to the remaining inert fiberglass mesh, which acts as a flashback arrestor, the extinguished side was not able to be reignited by the remaining flame. The remaining flame would then shrink in length due to the reduced heat transfer to the solid to a shorter length. The one-sided flame will spread stably with a constant speed and a constant flame length to the end of the sample. A constant length flame implies that the pyrolysis front and the burnt out fronts move at the same speed. For the wider samples (. 7cm), no one-sided extinction is observed. Two-sided flames spread all the way to the top of the sample. For these wider widths, the flames are still growing and have not reached their limiting length if it exists. Care was taken to minimize the amount of non-symmetries in the experimental configuration. Repeated tests show that blow-off can occur on either side of the sample. The flame growth is observed to be very symmetric during the growth phase and grew to significant length (>10cm) before extinction of the flame on one side. Our proposed explanation of this unusual phenomenon (i.e. stronger two ]sided flame cannot exist but weaker one-sided flame can) is as follows: The observed one-sided extinction is a blow- off induced by buoyant entrainment. It is known that the flammable diffusion flame regime is bounded by quenching and blow ]off limits when varying incoming air velocity. The narrowest samples tested (between 2 and 5 cm) begin within the flammable range, but as the flame grows, the buoyancy driven air velocity increases at the neighborhood of the flame base. The initially stable flame crosses the extinguishment boundary resulting in a flame blow-off. When one-side of the flame extinguishes, the remaining side shrinks due to the reduced heat transfer to the solid. This reduces the induced velocity and the flame becomes stable. It is proposed that this may have implications to upward flame growth beyond this experiment.
[发布日期] 2013-03-16 [发布机构]
[效力级别] [学科分类] 力学,机械学
[关键词] [时效性]