Interface Horizontal Shear Strength in Composite Decks With Precast Concrete Panels
[摘要]

Six stay-in-place precast, prestressed deck panels were tested to evaluate the horizontal shear strength between the precast panel and the cast-in-place portion of the bridge deck. Presently, the Indiana  Department of Transportation requires a minimum of 20 shear connectors regardless of panel dimensions. The shear connectors are placed across a broom finished deck panel surface. Broom finish with  approximately 0.05 to 0.075 in. (1 .27 to 1.91 mm) total amplitude deformations is specified instead of a raked finish with 0.25 in. (6.35 mm) total amplitude because of the reduced 2.5 in. (63.5 mm) thickness of the panels used in Indiana. In this study, composite behavior at ultimate, including horizontal shear and interface slip characteristics, was evaluated. It is concluded that stay-in-place precast,  prestressed deck panels with a broom finished surface do not require horizontal shear connectors if the nominal average horizontal shear stress at the interface is less than 116 psi (0.8 MPa).

[发布日期]  [发布机构] 
[效力级别]  [学科分类] 建筑学
[关键词]  [时效性] 
   浏览次数:2      统一登录查看全文      激活码登录查看全文