Impact Toughness of Steel WMD After TIG Welding
[摘要] The material selected for this investigation was low alloy weld metal deposit after TIG welding with various amount of oxygen in weld metal deposit (WMD). After TIG process it is difficult to get proper amount of oxygen in WMD on the level much lower than 350 ppm. The highest impact toughness of low alloy WMD corresponds with the amount of oxygen in WMD above 350 ppm. In the paper focuses on low alloy steel after innovate welding method with micro-jet cooling that could be treated as a chance on rising amount of oxygen in weld. Weld metal deposit (WMD) was carried out for TIG welding with micro-jet cooling with various amount of oxygen in WMD. In that paper various gas mixtures (gas mixtures Ar-O2 and Ar-CO2) were tested for micro-jet cooling after TIG welding. An important role in the interpretation of the results can give methods of artificial intelligence.
[发布日期]  [发布机构] 
[效力级别]  [学科分类] 金属与冶金
[关键词] Industrial Chemistry;Substances and Products;Materials Sciences;Materials Processing [时效性] 
   浏览次数:2      统一登录查看全文      激活码登录查看全文