Effect of Liquid Penetrant Sensitivity on Probability of Detection
[摘要] The objective of the task is to investigate the effect of liquid penetrant sensitivity level on probability of detection (POD) of cracks in various metals. NASA-STD-5009 currently requires the use of only sensitivity level 4 liquid penetrants for NASA Standard Level inspections. This requirement is based on the fact that the data used to establish the reliably detectable flaw sizes penetrant inspection was from studies performed in the 1970s using penetrant deemed to be equivalent only to modern day sensitivity level 4 penetrants. However, many NDE contractors supporting NASA Centers routinely use sensitivity level 3 penetrants. Because of the new NASA-STD-5009 requirement, these contractors will have to either shift to sensitivity level 4 penetrants or perform formal POD demonstration tests to qualify their existing process. We propose a study to compare the POD generated for two penetrant manufactures, Sherwin and Magnaflux, and for the two most common penetrant inspection methods, water washable and post emulsifiable, hydrophilic. NDE vendors local to GSFC will be employed. A total of six inspectors will inspect a set of crack panels with a broad range of fatigue crack sizes. Each inspector will perform eight inspections of the panel set using the combination of methods and sensitivity levels described above. At least one inspector will also perform multiple inspections using a fixed technique to investigate repeatability. The hit/miss data sets will be evaluated using both the NASA generated DOEPOD software and the MIL-STD-1823 software.
[发布日期] 2011-01-01 [发布机构]
[效力级别] [学科分类] 金属与冶金
[关键词] [时效性]